Polyether series: injection grade, extrusion grade
Applicable processing methods: injection grade, extrusion grade
Product features: low temperature resistance, easy processing, anti-bacterial resistance, good physical properties, hydrolysis
Applicable products: sports equipment, pipe, industrial supplies, round timber, medical equipment, other
Physical properties of speciesTest methodsUnitPU 80AGPU 85AGPU 90AGPU 95AGPU 98AGPU 64DIGPU 71DIGPU 74DIG
ProportionASTM D792 kg/cm21.10±0.021.10±0.021.14±0.021.14±0.021.16±0.021.16±0.051.16±0.051.16±0.02
HardnessASTM D2240 Shore A Shore D82A±2 32D±285A±2 40D±290A±2 45D±295A±2 50D±297A±2 54D±298A±2 63D±299A±2 68D±299A±2 72D±2
100% ModulsASTM D412 kg/cm250±1560±1580±15110±15150±15200±15260±15210±15
300% ModulsASTM D412 kg/cm280±15100±15110±15140±15230±15280±15370±15310±15
Tensile strengthASTM D412 kg/cm2260±100300±100320±100350±100400±100450±100400±100350±100
ElongationASTM D412 %700±100550±100530±100530±100500±100500±100300±100380±100
Tear strengthASTM D624 kg/cm270±1580±1590±15110±15130±15180±15150±15150±15
Abrasion resistanceDIN53516mm380±1580±1560±1560±1590±1590±1590±15100±15
Compression ratio 70°Cx22hrsASTM D395%        
properties  TransparentTransparentTransparentTransparentTransparentTransparentTransparentTransparent
Shrinkage %2.2~2.8%2.2~2.8%2.2~2.8%1.5~2%1.5~2%1.5~2%1.5~2%1.5~2%
Remarks1 The above data for reference only, the actual value due to detection test piece thickness varies slightly different specifications 2 recommended drying temperature: 90 ° C ~ 110 ° C room, drying time 3-4 hours 3 Packing 25KG / bag (can use color bag or empty bag to customer needs).